Why Ms matters in welding and heat treatment
Holding a weld above Ms until hydrogen has diffused out, or until the transformation is controlled, reduces cold cracking in hardenable steels. In heat treatment, a low Ms means more retained austenite and greater distortion risk.
Accuracy
Empirical equations like this are typically within about ±25 °C for the steels they were fitted to. Austenitising conditions and grain size also affect Ms, so use dilatometry where precision matters.
Assumptions and limits
- Fully austenitised before cooling, all alloying in solution.
- Composition within the range of the Andrews data set.
References
- Andrews, K. W., Empirical formulae for the calculation of some transformation temperatures, JISI, 1965.
- Koistinen, D. P. and Marburger, R. E., Acta Metallurgica, 1959.
Questions
- What is the Ms of 4140 steel?
- Around 320 to 340 °C, depending on the exact analysis. Enter the heat analysis for a better estimate.
- Does silicon affect Ms?
- Only weakly; the Andrews linear equation leaves it out.
This calculator is a design aid. Check results against the governing code or standard and have critical work verified by a qualified engineer. Read the disclaimer.