Typical values
Annealed austenitic stainless steels have n around 0.4 to 0.5, low-carbon deep-drawing steels around 0.2 to 0.25, and high-strength steels 0.1 or less. By Considère's criterion, necking begins when true strain equals n.
Better accuracy
Two points give an estimate. ISO 10275 and ASTM E646 fit a straight line through many points on a log-log plot between defined strain limits.
Assumptions and limits
- Material follows a power law between the two points.
- True stress and true strain, not engineering values.
References
- Hollomon, J. H., Tensile deformation, Trans. AIME, 1945.
- ASTM E646 and ISO 10275, tensile strain-hardening exponents.
Questions
- Can I use engineering stress and strain?
- Convert them first with the true stress and strain calculator; the Hollomon equation is defined in true values.
- What is a good n for deep drawing?
- Higher is better for stretch forming; drawability depends more on the Lankford r-value.
This calculator is a design aid. Check results against the governing code or standard and have critical work verified by a qualified engineer. Read the disclaimer.