PREN Calculator (Pitting Resistance Equivalent Number)

PREN ranks stainless steels by their resistance to pitting corrosion in chloride environments such as seawater. It is a weighted sum of chromium, molybdenum, tungsten and nitrogen content, so a higher number means better pitting resistance.

Inputs

wt%
wt%
wt%
Advanced options (2)
wt%

Results

PREN
35.5
PREN without W
35.5
Similar to
2205 duplex (typical PREN about 35)

    RefENG-MAT-002
    MethodPREN = Cr + 3.3(Mo + 0.5W) + 16N
    UnitsSI
    Date2026-11-23

    Working

    Calculated in SI base units; inputs are converted from the units you choose.

    1. Pitting resistance equivalent numberPREN = Cr + 3.3(Mo + 0.5W) + 16NPREN = 22.5 + 3.3 × (3.1 + 0.5 × 0) + 16 × 0.17 = 35.45

    Typical PREN of common grades (minimum composition basis varies)

    GradeTypical PREN
    304 / 304L19
    316 / 316L24
    2304 lean duplex26
    2205 duplex35
    904L35
    2507 super duplex42
    6Mo super austenitic (254 SMO)43

    Where PREN is used

    Material specifications for offshore, desalination and chemical plant often set a minimum PREN, for example 40 or more for super duplex grades. Checking an actual heat analysis against that minimum is a routine part of material verification.

    Limits of the index

    PREN reflects composition only. Real pitting resistance also depends on microstructure, surface finish, temperature, weld quality and the absence of intermetallic phases, so two materials with the same PREN can behave differently in service. Use the index to compare and screen alloys, not to predict corrosion life.

    Assumptions and limits

    • Composition in weight percent.
    • Nitrogen factor 16 unless changed.

    References

    • ISO 15156-3, Materials for use in H2S-containing environments (PREN definitions).
    • ASTM A923 and NORSOK M-001 material requirements referencing PREN.

    Questions

    What PREN is needed for seawater?
    Grades with a PREN of 40 or more, such as super duplex 2507 or 6Mo austenitic steels, are generally chosen for seawater service. 316L (about 24) is prone to pitting in warm seawater.
    Should I use 16 or 30 for nitrogen?
    Use whatever your specification states. 16 is the most common factor; 30 is sometimes used for austenitic grades, where nitrogen has a stronger effect.

    This calculator is a design aid. Check results against the governing code or standard and have critical work verified by a qualified engineer. Read the disclaimer.