Brinell and Vickers Hardness from Indentation

Enter the test force and the measured indentation to get Brinell or Vickers hardness. The calculator applies the standard definitions, so it is useful for checking a hardness tester, working out values from a microscope measurement or recording results for a test report.

Inputs

Results

Hardness
228.8
Designation
229 HBW 10/3000
Mean indentation size
4

    RefENG-MAT-005
    MethodHBW = 0.102·2F/(πD(D − √(D² − d²))); HV = 0.1891·F/d²
    UnitsSI
    Date2026-11-23

    Working

    Calculated in SI base units; inputs are converted from the units you choose.

    1. Mean indentation diameterd = (d1 + d2)/2 = 4 mm
    2. Brinell hardness (F in N, D and d in mm)HBW = 0.102 × 2F / (πD(D − √(D² − d²)))HBW = 0.102 × 2 × 29,420 / (π × 10 × (10 − √(10² − 4²))) = 228.8

    Brinell test

    A tungsten carbide ball is pressed into the surface and the diameter of the impression is measured in two directions. Hardness is force divided by the curved surface area of the impression. Common combinations are a 10 mm ball with 3000 kgf for steel and 500 or 1000 kgf for softer metals. The result is only valid when the impression is between 0.24 and 0.6 times the ball diameter.

    Vickers test

    A square-based diamond pyramid with a 136° angle between faces is used, and both diagonals of the impression are measured. Because the impression is geometrically similar at any load, Vickers values are largely independent of force, which makes the method suitable for thin sections, coatings and weld traverses.

    Assumptions and limits

    • Test force in newtons for the formulas; kgf is converted using g = 9.80665 m/s².
    • Indentation measured in millimetres.

    References

    • ISO 6506-1, Metallic materials: Brinell hardness test.
    • ISO 6507-1, Metallic materials: Vickers hardness test.
    • ASTM E10 and ASTM E384.

    Questions

    Why is my Brinell result flagged as invalid?
    If the impression is too small or too large relative to the ball, the result depends on the test conditions. Choose a force-to-diameter ratio that keeps d between 0.24D and 0.6D.
    Can I convert HV to HRC here?
    Not on this page. Conversions between scales are empirical and depend on the material; they will be covered by a separate hardness conversion calculator.

    This calculator is a design aid. Check results against the governing code or standard and have critical work verified by a qualified engineer. Read the disclaimer.