Recovery
Not all of the element in the ferroalloy ends up in the metal; some oxidises into the slag. Recovery depends on the element, deoxidation state, temperature and addition practice. Manganese and silicon recoveries of 80 to 95% are common in ladle additions; nickel and molybdenum are close to 100%.
Checking the result
After the addition and stirring, take a sample and confirm the analysis with an optical emission spectrometer before tapping or casting.
Assumptions and limits
- Element fully dissolved and mixed.
- Recovery as entered.
References
- Standard foundry and steelmaking charge calculation practice.
Questions
- Why not just use M × (ct − c0) / a?
- That ignores recovery and the dilution caused by the added mass. The difference is small for small additions but grows for large adjustments.
- Can I lower an element with this?
- No. To lower content, dilute with a low-alloy charge; this calculator handles additions only.
This calculator is a design aid. Check results against the governing code or standard and have critical work verified by a qualified engineer. Read the disclaimer.